本文二维码信息
二维码(扫一下试试看!)
脱油樟木APMP制浆性能研究
Study on APMP Pulping Property of De-oiled Camphor Woodchips
投稿时间:2023-12-18  
DOI:10.11980/j.issn.0254-508X.2024.05.008
关键词:  樟木  APMP制浆  物理性能  H2O2漂白  COD
Key Words:camphor woodchips  APMP pulping  physical properties  H2O2 bleaching  COD
基金项目:
作者单位邮编
银辉 岳阳林纸股份有限公司工程技术研究中心湖南岳阳414000 414000
朱宏伟* 岳阳林纸股份有限公司工程技术研究中心湖南岳阳414000 414000
阳路 岳阳林纸股份有限公司工程技术研究中心湖南岳阳414000 414000
林本平 长沙理工大学 化学化工学院湖南长沙410004 410004
刘永丰 岳阳林纸股份有限公司工程技术研究中心湖南岳阳414000 414000
赵靖 岳阳林纸股份有限公司工程技术研究中心湖南岳阳414000 414000
邓凤伟 岳阳林纸股份有限公司工程技术研究中心湖南岳阳414000 414000
李丹 岳阳林纸股份有限公司工程技术研究中心湖南岳阳414000 414000
谢正文 岳阳林纸股份有限公司工程技术研究中心湖南岳阳414000 414000
摘要点击次数: 794
全文下载次数: 601
摘要:分析了蒸汽脱油后樟木片的材性和化学组分,实验室和工厂中试评估了该原料APMP制浆性能并分析了制浆过程中的废水负荷情况,探讨了樟木APMP浆碱性H2O2漂白的可漂性能。结果表明,在漂白温度90 ℃、浆浓25%、NaOH用量60 kg/t浆、H2O2 50 kg/t浆条件下,樟木APMP浆的物理强度略低于杨木APMP浆、高于桉木APMP浆,可漂性低于杨木APMP浆和桉木APMP浆,樟木APMP制浆过程废水总COD负荷为杨木、桉木的2倍,当H2O2用量70 kg/t浆时,樟木APMP浆白度可达75.0%,得率82.5%。微漂APMP制浆中试结果表明,当H2O2用量27 kg/t浆时,樟木APMP浆白度达35.9%。在打浆度44.0 °SR时,纸张抗张指数达28.5 N·m/g,松厚度2.57 cm3/g,可用于配抄中高端包装纸产品。
Abstract:Chemical components of de-oiled camphor woodchips were analyzed. Laboratory and pilot scale trials on APMP pulping properties of de-oiled camphor woodchips were performed.The bleaching property of alkalire H2O2 of de-oiled camphor wood APMP pulp was investigated. The results showed that under the conditions of NaOH dosage 60 kg/t pulp, H2O2 dosage 50 kg/t pulp, temperature 90 ℃ and pulp consistency 25%, physic strengths of camphor wood APMP pulp were higher than eucalypt APMP pulp, but lower than poplar APMP pulp, however its bleachability was lower than both above. In terms of total COD of wastewater, the APMP pulping process of camphor wood was twice that of poplar wood and eucalyptus wood. As the H2O2 dosage of 70 kg/t pulp, camphor pulps could be produced at a brightness level of 75.0% with a yield of 82.5%. Results of pilot trials of camphor woodchips chemimechanical pulping showed that, at the H2O2 dosage of 27 kg/t pulp, camphor woodchips APMP pulps were produced with a brightness of 35.9%. Papers were prepared from camphor woodchips APMP pulp at beating degree of 44.0 °SR, with tensile strength of 28.5 N·m/g and bulk of 2.57 cm3/g, which was acceptable as furnish for mid-high grade of packaging papers.